Brand Name: | Esun |
Model Number: | ES1703-1 |
MOQ: | 4rolls 0.075mm*30cm*100m&2rolls 0.075mm*60cm*100m |
Price: | Negotiable |
Payment Terms: | T/T, paypal |
Supply Ability: | 3000meters per day |
Single Double Side Matte Surface DTF PET Film Roll 75U 30cm 33cm 60cm
Single Double Side Matte 75U 30cm 33cm 60cm Dtf Film Roll Dtf Pet Film
Dtf Pet Film Product Description
PET printing film is also called color inkjet film, digital printing film and so on. The water-based colored ink and white ink are directly printed on the printing film through the printer to form various beautiful patterns, which are dried by sprinkling hot melt adhesive powder and then transferred to the ironing object.
It is easy to peel off. The pattern after ironing is bright in color, soft to the touch, good elasticity, washable, rubbing resistance, hand-washed and machine washable, strong weather resistance, high and low temperature The glue will not open or break under the environment.
We have single side and double side with hot peeling and cold peeling
Single Side: Matte Side Is The Printing Side Glossy Side Is Non-printing Side.
Double Sided: The Printing Surface Coating Can Be Buckled Off, The Other Side Cannot Be Buckled Off .
Dtf Pet Film Product Specification:
Product Specification |
Conventional Thickness |
0.075mm |
|
Conventional Length |
100m |
|
Conventional Width |
600mm |
|
Finished Product |
0.075mm*600mm*100m/roll |
Washing Resistance |
Washable Temperature |
45℃-60℃ |
Storage Conditions & Shelf Life |
It is strictly forbidden to collide with sharp objects. When opening the package and not using it, please seal it and store it to prevent moisture and high temperature |
|
|
The storage conditions are temperature -5℃-30℃, humidity 40-80%, avoid direct sunlight, shelf life is one year |
Dtf Pet Film Operating Conditions
THE heat press temperature is 150℃-160℃,and the heat press time is 8-15 seconds with pressure 0.3-0.5mpa
Cautions:
1. Tear-off method: cool tear or hot tear.
2. The printing film is a soft product. A slight stickiness on the surface is normal, and the surfaces should be prevented from sticking to each other.
3. Reasonably control the temperature and pressing time. If the temperature is too high or the time is too long, it will easily cause discoloration or decrease in elasticity
FAQ
Q1) . How about your MOQ of PET printed film?
2rolls 0.075mm*30cm*100m 1roll 0.075mm*60cm*100m
1500 sheets A3
3000 sheets A4
We can do 30cm, 32cm, 40cm, 50cm, 60cm, 61cm, 100.5cm, 110cm, 120cm, 122cm.
Product specifications can be customized.
Q2). how can we guarantee quality?
Always a pre-production sample before mass production;
Always final Inspection before shipment;