75 Micron DTF Printing Film Single Sided Matte PET Film Rolls
Keywords | DTF Printing Film | Conventional Thickness | 0.075mm |
---|---|---|---|
Conventional Width | 600mm | Finished Product | 0.075mm*600mm*100m/roll |
Heat Press Temperature | 130℃-160℃ | Washable Temperature | 45℃-60℃ |
Package | 2rolls Per Carton | Shape | Roll |
High Light | 75 Micron DTF Printing Film,Single Matte DTF Printing Film,75 Micron PET Film Roll |
75 Micron DTF Printing Film Single Sided Matte PET Film Roll
DTF Printing Film Description
The DTF PET Transfer Film is a single-sided printing film suitable for all kinds of textile fabrics. It is easy to peel off. The pattern after ironing is bright in color, soft to the touch, good elasticity, washable, rubbing resistance, hand-washed and machine washable, strong weather resistance, high and low temperature The glue will not open or break under the environment.
DTF Printing Film Physical Characteristics:
Product Specification |
Conventional Thickness | 0.075mm, 0.10mm |
Conventional Length | 100m | |
Conventional Width | 600mm | |
Finished Product | 0.075mm*600mm*100m/roll | |
Operating Conditions | Heat Press Temperature | 130℃-160℃ |
Heat Press Time | 8-15 seconds | |
Pressure | 0.3-0.5mpa | |
Washing Resistance | Washable Temperature | 45℃-60℃ |
Storage Conditions & Shelf Life | It is strictly forbidden to collide with sharp objects. When opening the package and not using it, please seal it and store it to prevent moisture and high temperature | |
The storage conditions are temperature -5℃-30℃, humidity 40-80%, avoid direct sunlight, shelf life is one year |
Cautions:
1. Tear-off method: cool tear or hot tear.
2. The printing film is a soft product. A slight stickiness on the surface is normal, and the surfaces should be prevented from sticking to each other.
3. Reasonably control the temperature and pressing time. If the temperature is too high or the time is too long, it will easily cause discoloration or a decrease in elasticity
DTF Printing Film Applications